Property | Levapor |
---|---|
Material | Reticulated Poly Ether based PU Foam impregnated with activated carbon |
Individual Cube Size | 20 * 20 * 7 mm |
Weight of media | 25 kg /m3 (Dry Weight), 65-80 kg / dump m3 of colonized carriers |
Surface Area | > 20,000 m2 / m3 |
Sp. Gravity | 1.02 to 1.08g / cm3 |
Porosity | > 90 % |
Degree of Reactor Filling Required | 10 – 15 % |
Full Fluidization energy | 4 – 7 Nm3 / m2.hr air |
Wetting Period | 1 – 3 days |
Colonization | 60 – 90 minutes |
Author Bio
Amit Christian is a MSc graduate in Environment Science from Middlesex University, London, UK. He has been active in the field of water and wastewater treatment since 1998. He specializes in design, engineering, and management of various biological wastewater treatments such as Activated Sludge Process (ASP), Sequencing Batch Reactor (SBR), Moving Bed Bio Reactor (MBBR), Integrated Fixed Film Activated Sludge (IFAS). He has helped various Industrial and Municipal clients in troubleshooting , optimizing their biological wastewater treatment processes to achieve latest Stringent norms for Ammonia Removal.